Home > PRODUCTS > Finishing Materials > Interiors
BTS Marble Marble Plus Pearl Shining
Fine Stone Embossing coat AG CERAMIC COAT
BTS (Baroco Triple System) Travertine  
 

Water-soluble interior finish product using special synthetic resin, quartz sand and pigment expressing the color and texture of luxurious expensive marble It is suitable for interior finish material owing to excellent non-toxicity, non-flammability, pollution-resistance, wash ability and durability.

 
Application

APT specialization: elevator hall, stairs, inner wall of corridor, ceiling and others
Commercial building: inner wall and ceiling of quality cafeteria, hotel, condominium and entertainment shops
Art facilities: inner wall and ceiling of premium exhibition hall, multipurpose hall, gallery and concert hall.

 
Construction Method

1. Completely remove out any foreign materials, such as dust, oil, or water.
2. Repair small cracks, grooves, or damaged parts with Baro Putty.
3. Apply the color primer, which is in the same color as the lining material, to the surface, using a roller or a spray.
4. In case the color primer work is not done, the phenomenon of whitening or difference in the finishing color can happen so it should be done before the finishing work.
5. Be sure to do the curing work in advance in order to prevent any finishing material from flying out.
6. After the primer work is completely dry, adjust the air pressure of the compressor and the nozzle diameter of the spray suitably for the construction pattern, input a finishing material, and try a preliminary test to make the pattern that you want.
7. Put Marble Plus into the gun, adjust the air pressure of the compressor, and apply on the whole in the thickness of 1.5mm for small particle-patterns.
8. The minimum thickness of one-time coating should not be more than 1.5mm. In case it is thick, cracks can be made.
9. After making spray patterns, make patterns in a certain direction, using an unpolluted trowel or a flat spoon.
10. You should do the work in one direction to have the consistent texture of the patterns.
11. The spray work and the following work (patterning) should be done consecutively.
12. Check whether the surface is dry or not after it is cured for 24 hours.
13. The temperature, humidity, and wind of a jobsite can make a difference.
14. In order to maintain the smoothness of the surface, do the primary polishing work (#100 electric sander or air sander).
15. The polishing work should be done before it becomes completely dry. In general, it is suitable to complete the polishing work within 12~ 36 hours after the construction work.
A type: Use #800 or higher polishing paper to make it naturally glossy.
B type: Evenly spray a transparent coating material (glossy, flat) for final finishing.
It is a principle that a spray is used for coating, and in case you want to make any other special finishing effect, please contact us.

 
Attention for the construction work

1. The temperature for the construction work should be over 5 ° C and the humidity should be less than 80%.
2. The drying work takes long time so before doing the finishing work, be sure to check the weather first. In case it is difficult to work further because of rain, immediately take a curing action for the existing applied surface which is not dry yet in order to prevent it from being damaged.
3. Protect the finishing material from any pollutants floating in the air, like dust and smoke, and from weather (less than 5 ° C temperature; over 80% humidity) until it becomes dry.
4. Remove the white part of the concrete surface in advance, and do the construction work when it is completely cured.
5. Repair any polluted or damaged part and do the construction work again.
6. In case it is judged that the pattern has a problem, stop the work, remove out the problem, take corrective actions for the causes, and then, work.
7. For the repair work, completely remove any pollutants from the existing walls, reinforce the surface with Baro Primer, and then, do the work.
8. For the surface that is not cured after the mesh finishing or the cement mortar finishing work, don’t do the construction work.
9. don’t do the construction work on the bottom surface that is coated with oil or asphalt.
10. Do not mix with other paints.
11. Prepare sufficient labor and equipment for consecutive works, and be careful not to have working joints or quality change.
12. Keep all the materials in the place which is out of the direct rays of the sun and well-ventilated (a dry, cool, and dark place in the temperature of 5° C~30 ° C).
13. In case you have to stop the work while doing the lining work, be careful not to make any spray joint.

 
Special Remark
Item Construction Method Construction
Area (pail)
Drying Time Packing Unit
Marble Plus Spray 12-15 m² Over 48 hours 25kg/pail
 
PROCESSING FLOW CHART
Process Materials Mixture
(Weight
Ratio)
Consumption
(kg/m²)
Painting Frequency Time Interval (HR) Method
In process Between
process
Final Curing  
Base
Coating
Completely remove impurities in the lower part.
Make even the surface with grooves,cracks, and fractures with the putty.
Under
Coating
Primer 100 0.2-0.4 1   Over 24   Brush,
roller,
Spray
Second
Coating
Marble Plus 100 2-3 Over 1   Over 48  

Air
Mortar
Gun
Diameter
5-6mm
Pressure
3-5kg/

Top
Coating
Barotop 1000 100 0.2-0.4 2     Over 4 Spray
Tap Water 5-10            
 
Property
Category Result Remark
Composition Type 1 Water-soluble  
Specific Gravity 1.6±0.05  
Solid Volume Ratio 80±1%  
Viscosity 80,000±5,000CPS  
pH 7.5±0.5  
Coverage 2.5±0.5 ㎏/㎡  
Coating Thickness 0.8 ~ 1.5㎜  
Drying Time Less than 72 hrs Temp over 20℃,
Humidity lower than 80%
Packing Unit 25㎏/PL