Home > PRODUCTS > Finishing Materials > Exterior Use
Triple stone Geny Stone V Chip Stone
Modern Stone Shine Stone Prime Stone
Bella Stone Stucco Baro Coat (EIFS)
 

With premium pigment, it may express vivid color and texture with more reasonable price than Triple stone and be applied to any interior or exterior regions of a building.
In addition, itis expected that its excellent water-resistance, durability, anti-flammability and anti-discoloration may improve a buildings value.

 
Construction Method

1. Remove out any dust, floating matters, and foreign materials on the surface.
2. Do the repair work for the cracks or the damaged parts of the surface, using Baro Putty, to make the surface smooth.
3. Apply Baro Primer to the whole surface, using a roller or a spray, to strengthen the adhesiveness.
4. Discuss PVC joint sealant and joint interval with the owner of a building in advance prior to the construction work.
5. Strongly adhere the joint sealant by use of a caulking material so that the joint sealant won’t fall off.
6. Remove the joint sealant cover after spraying Geny Stone.
7. You can mix a hardener for curing and workability on a jobsite
8. Do the necessary curing work in advance to prevent a finishing material from flying out.
9. Use a spray gun to apply. The nozzle diameter for the spray gun should be 6-10mm and its pressure for use should be 3-5kgf/cm².
10. During the Geny Stone spraying work, the color and the pattern can become different so test it in advance.
11. Do the construction work after the color primer-applied surface is completely cured. When using a spray gun, be sure to make the right angle (90°) on the surface.
12. Put Geny Stone into a BTS gun and apply it on the whole in the thickness of 1.5mm for small particle-patterns.
13. As the product may be applied too thickly or thinly, make sure to maintain a constant speed and be careful to prevent metamerism in the duplicated part.
14. Before getting dry on the surface after spraying, apply light oil or white kerosene on the construction area using a roller. (Do not give too strong pressure for natural patterning.)
15. 12 hours later, check the dryness conditions of the surface.
16. After roller work is completed and the surface is completely dried, apply a coating material to the surface, using a roller or a spray.
17. In case you have to stop the work in the middle, be careful not to make any spray joint.
18. Be sure to protect the whole surface until it is dried dry after the work is done.

 
Attention for the construction work

1. The temperature for the construction work should be over 5°C and the humidity should be less than 80%.
2.The curing work takes long time so before doing the finishing work, be sure to check the weather first. In case it is difficult to work further because of rain, immediately take a curing action for the existing applied surface which is not dry yet in order to prevent it from being damaged.
3. Protect the finishing material from any pollutants floating in the air, like dust and smoke, and from weather (less than 5°C temperature; over 80% humidity) until it becomes dry.
4. Remove the white part of the concrete surface in advance, and do the construction work when it is completely dry.
5. Repair any polluted or damaged part and do the construction work again.
6. In case it is judged that the pattern has a problem, stop the work, remove out the problem, take corrective actions for the causes, and then, work.
7. For the repair work, completely remove any pollutants from the existing walls, reinforce the surface with Color Primer, and then, do the work.
8. For the surface that is not cured after the mesh finishing or the cement mortar finishing work, Don’t do the construction work.
9. Don’t do the construction work on the bottom surface that is coated with oil or asphalt.
10. Do not mix with other paints.
11. Prepare sufficient labor and equipment for consecutive works, and be careful not to have working joints or quality change.
12. Keep all the materials in the place which is out of the direct rays of the sun and well-ventilated (a dry, cool, and dark place in the temperature of 5°C ~ 30°C).
13. In case you have to stop the work while doing the lining work, be careful not to make any spray joint.

 
Special Remark
Classification Painting Method Coverage (Bin) Drying Time Packing Unit
Geny Stone Spray 8-10m² Over 48 hours 25kg / Pail
 
PROCESSING FLOW CHART
Process Materials Mixture
(Weight
Ratio)
Consumption
(kg/m²)
Painting Frequency Time Interval (HR) Method
In process Between
process
Final Curing  
Base
Coating
Completely remove impurities in the lower part.
Make even the surface with grooves,cracks, and fractures with the putty.
Under
Coating
Primer 100 0.2-0.4 1   Over 24   Brush,
roller,
Spray
Joints Line drawing Design the location of joints and draw lines using inking lines or chalk.
Joint work

Attach joints on lines marked in a designated space using corking agents.
Remove the cover of joints after second coating.

Second
Coating
Geny Stone 100 3-5 2   Over 48  

BTS Gun
Diameter
6-10 mm
Pressure
3-5kg/

Top
Coating
Barotop 1000 100 0.2-0.4 2     Over 4 Brush,
roller,
Spray
Tap Water 5-10            
 
Property
Category Result Remark
Composition Type 1 Water-soluble  
Specific Gravity 1.6±0.5  
Solid Volume Ratio 81±1%  
Viscosity CPS  
pH 8±0.5  
Coverage 8-10 ㎏/㎡  
Coating Thickness 1.5~2㎜  
Drying Time 48 hrs  
Packing Unit 25kg / Pail  
 
Application

- APT specialization( main entrance, an outer wall, pilotis & inner/outer spraying finish material)
- The highest grade inner/outer finish for APT/business center/residence